Do you have any formal reference of what the ideal pin adhesion test result should be.   For agro boxes (vegetables) we currently use values of 55 to 60  (pound/inch) and in industrial 40 and higher.

We have a particular customer that has experienced some delamination failures. The PAT test value is 27 (pound/inch) which we believe to be too low. However, we are lacking established information to back up our opinion.

I could not agree with you more.  I prefer a minimum, not average, of 45 for industrial application.  My technical associates at TAPPI like this 45 value while I would rather have 55 on all corrugated bonds.  It is most important to know where the failure is occurring: linerboard, medium, or in the starch itself.  Under ideal conditions we want 100% liner failure. As you can see in these photos a very low PAT value can have disastrous results. There is very little liner pull and very little glue with a poor bond.

A good reference for the PAT is the most recent version of TAPPI document TM 821 (TM 821-0M 17 at this writing), Pin adhesion of corrugated board by selective separation.

— Ralph

Pin Adhesion Test sample Pin Adhesion Test sample Pin Adhesion Test sample

Leave a Reply

Please log in using one of these methods to post your comment:

WordPress.com Logo

You are commenting using your WordPress.com account. Log Out /  Change )

Google photo

You are commenting using your Google account. Log Out /  Change )

Twitter picture

You are commenting using your Twitter account. Log Out /  Change )

Facebook photo

You are commenting using your Facebook account. Log Out /  Change )

Connecting to %s

This site uses Akismet to reduce spam. Learn how your comment data is processed.


%d bloggers like this: